Peculiarity:
The grinding speed is fast, the heat dissipation is fast, and the polishing effect is good. (No water cooling required!)
Step:
1) Ceramic grinding head for maxillofacial and adjacent dressing (speed 15000-20000/min)
2) The gray-white grinding head is used for leveling and pre-polishing (speed 10000-15000/min)
3) Yellow grinding head for high-brightness polishing (speed 8000-12000/min)
Effect:
1) The special properties of ceramic diamond can quickly dress the post-crystallization cobalt oxide restoration without water cooling, which simplifies the complicated operation process of traditional diamond burs under water cooling
2) The special properties of rubber diamond can quickly achieve high-brightness polishing effect
Note: There is no need to apply too much pressure and use it at the recommended speed to avoid cracking of the restoration.
Page Copyright ©2021All Rights Reserved.Shanghai TOBOOM Technology Co., Ltd Powered by www.300.cn 沪ICP备2020028574号-1